***ALL WORK TO MATCH EXISTINGRef code GJ6UQT
Remove deteriorated floor boards, stringers, and fascia boards.
Install new 3"x4" beaded stringers, 5/4x4 wood T&G floorboards, and 7/8" fascia with ½" bead, all as per VCC Standard Detail Sheet No. 12 (attached).
PAINT TO MATCH
Remove all vegetation from exterior walls.
To repoint masonry utilizing mortar mixed and applied per the VCC standard detail sheet (attached)
Any deteriorated, cracked, or broken bricks shall be replaced to match existing in color, size, material, porosity, detail, profile and exposure.
All reinstalled masonry must be properly "toothed in" to existing masonry wall, using VCC mortar formula (attached).
VOIDS IN THE BRICK ARE NOT TO BE FILLED WITH MORTAR. BROKEN, DETERIORATED BRICKS MUST BE REPLACED WITH BRICKS MATCHING THE PREVIOUS.
All mortar to be mixed using the VCC recipe (attached) with a maximum of 1 part Portland Cement, to 3 parts lime, to 9 parts sand, and enough water to form a workable mix. Prepackaged mixes are not permitted. The resulting mix should range in color from off-white to beige but should not be grey or white in color.
MORTAR IS NOT TO BE APPLIED OVER THE FACE OF THE BRICKS UNDER ANY CIRCUMSTANCES.
Doing so will result in a STOP WORK ORDER being placed on the property and violation case will be opened on the property.